Challenges
Datasets
Workspaces
Papers
Discussions
Leaderboard
Log inSign up
Challenges
Datasets
Workspaces
Papers
Discussions
Leaderboard
Blog
Job Board
Q3AS

© 2026 Aqora Quantum S.A.S.

TermsPrivacyLegal Notice

arXiv:2611.15021

Reducing TLS Losses in Superconducting Circuits Using Solid Neon

A. Palmer, K. Matkovic, P. Russell, E. Helgemo, L. Delventhal, Y. Ashlea Alava, K. Zuo, S.N. Coppersmith, M. C. Cassidy

Published Nov 11, 2026• 0 citations
arXivHTMLPDF

Abstract

Two level systems (TLSs) are a major source of loss in superconducting devices, limiting the performance of qubits, detectors, and resonators. These defects arise from a range of sources, including surface oxides, crystal defects, as well as fabrication residues which are often difficult to remove. Using NbTiN coplanar waveguide resonators, we show that depositing and subsequently removing a solid neon film can significantly improve device performance. Analysis of the temperature and power dependence indicates that this enhancement arises from reduced TLS dissipation, which we attribute to the redistribution and removal of surface contaminants during neon deposition and evaporation. Atomic force microscopy images of contaminated hexagonal boron nitride flakes before and after neon exposure show that neon treatment can redistribute and remove surface residues. These results demonstrate a simple, non-destructive approach for mitigating TLS losses in superconducting devices and other sensitive materials that cannot withstand aggressive cleaning processes.

DOI
10.48550/arxiv.2611.15021

Related papers

Reducing TLS loss in tantalum CPW resonators using titanium sacrificial layers

Zachary Degnan, Chun-Ching Chiu, Yi-Hsun Chen +5 more

We demonstrate a substantial reduction in two-level system loss in tantalum coplanar waveguide resonators fabricated on high-resistivity silicon substrates through the use of an ultrathin titanium sacrificial layer. A 0.2nm titanium film, deposited atop pre-sputtered α-tantalum, acts as a solid-state oxygen getter that chemically modifies the native Ta oxide at the metal-air interface. After device fabrication, the titanium layer is removed using buffered oxide etchant, leaving behind a chemically reduced Ta oxide surface. Subsequent high-vacuum annealing further suppresses two-level system loss. Resonators treated with this process exhibit internal quality factors Qi exceeding an average of 1.5 million in the single-photon regime across ten devices, over three times higher than otherwise identical devices lacking the titanium layer. These results highlight the critical role of interfacial oxide chemistry in superconducting loss and reinforce atomic-scale surface engineering as an effective approach to improving coherence in tantalum-based quantum circuits. The method is compatible with existing fabrication workflows applicable to tantalum films, offering a practical route to further extending T1 lifetimes in superconducting qubits.

quant-pharXiv:2601.16369•Applied Physics Reviews•Jan 26, 2026•4 citations

Enhanced superconducting qubit performance through ammonium fluoride etch

Cameron Kopas, Dominic P. Goronzy, Thang Pham +19 more

Abstract The performance of superconducting qubits is often limited by dissipation and two-level systems (TLS) losses. The dominant sources of these losses are believed to originate from amorphous materials and defects at interfaces and surfaces, likely as a result of fabrication processes or ambient exposure. Here, we explore a novel wet chemical surface treatment at the Josephson junction-substrate and the substrate-air interfaces by replacing a buffered oxide etch (BOE) cleaning process with one that uses hydrofluoric acid followed by aqueous ammonium fluoride. We show that the ammonium fluoride etch process results in a statistically significant improvement in median T 1 by ∼ 22 % (p = 0.002), and a reduction in the number of strongly-coupled TLS in the tunable frequency range. Microwave resonator measurements on samples treated with the ammonium fluoride etch after niobium deposition and etching also show ∼ 33 % lower TLS-induced loss tangent compared to the BOE treated samples. As the chemical treatment primarily modifies the Josephson junction-substrate interface and substrate-air interface, we perform targeted chemical and structural characterizations to examine materials differences at these interfaces and identify multiple microscopic changes that could contribute to decreased TLS losses.

arXiv:2408.02863•Materials for Quantum Technology•Oct 18, 2024•10 citations

Crystallinity in niobium oxides: A pathway to mitigate two-level-system defects in niobium three-dimensional resonators for quantum applications

Yasmine Kalboussi, I. Curci, F. Miserque +10 more

Materials imperfections in Nb -based superconducting quantum circuits—in particular, two-level-system (TLS) defects—are a major source of decoherence, ultimately limiting the performance of quantum computation and sensing. Thus, identifying and understanding the microscopic origin of possible TLS defects in these devices will help develop strategies that eliminate them, which are key to superconducting qubit performance improvement. In this paper, we demonstrate an order-of-magnitude reduction in two-level system losses in three-dimensional superconducting radio frequency (SRF) niobium resonators by a 10-h high vacuum (HV) heat treatment at 650 °C, even after exposure to air and high-pressure rinsing (HPR). X-ray photoelectron spectroscopy (XPS) and high-resolution scanning transmission electron microscopy (STEM) reveal an alteration of the native oxide composition regrown after air exposure and HPR and the creation of nanoscale crystalline oxide regions, which correlates with the measured tenfold quality factor enhancement at low fields of the 1.3 GHz niobium resonator. Tunneling spectroscopy measurements show a pronounced proximity effect that further confirms the presence of metallic layers on the niobium surface.

arXiv:2410.06805•Physical Review Applied•Apr 9, 2025•13 citations

Dielectric Loss in Superconducting NbN (200) CPW Resonator Developed on Si Substrate

Wei Qiu, Kazumasa Makise, Hirotaka Terai

In current superconducting qubit circuit development, coherence time is limited by low-frequency flux noise introduced from localized two-level systems (TLSs) in the fabricated superconducting circuit, including superconducting materials, the interface between thin films, and the substrate. As a part of the effect to tackle this issue from a substrate standpoint, we succeed in fabricating NbN (200) oriented coplanar waveguide resonator (CPWR) on a thin titanium nitride (TiN) (200) buffered Si (100) substrate. The internal loss is close to 3 × 10-5nearphoton> ~1, improved from ~2 × 10-4in NbN (200) CPWR fabricated on MgO (100). For NbN (200) resonators grown on Si (100), the internal loss shows microwave energy independent. To further clarity if this energy independence is due to the change of substrate material, we also fabricated TiN (200) CPWR on Si (100). In contrast to NbN (200) CPWR, the loss of TiN (200) resonator shows a strong microwave dependent, an indication of TLSs originated from the interface and the surface. We suggest TLSs in NbN (200) CPWR are dominated from different mechanism other than arising from the interface and surface.

IEEE Transactions on Applied Superconductivity•Jan 9, 2017•5 citations

Optimizing CMOS-compatible, superconducting titanium nitride resonators: Deposition conditions and structuring processes

Simon J. K. Lang, Alexandra Schewski, Ignaz Eisele +10 more

We report on the fabrication and characterization of superconducting coplanar waveguide (CPW) resonators based on titanium nitride (TiN) thin films deposited on 200\,mm diameter high-resistivity Si(100) substrates. We systematically investigate how deposition conditions, dry-etch power and in-situ resist strip temperature affect morphology, superconducting properties and dielectric losses. By tuning reactive sputtering conditions, three distinct preferred out-of-plane crystal orientations - (111), (200), and a mix of both are achieved. Our results demonstrate that all films exhibit similar minimal two-level system (TLS) losses, with TiN111 exhibiting the lowest median TLS losses $\tildeδ_\mathrm{TLS}$, and greater robustness against reoxidation. The applied structuring process, in contrast, has a far greater influence on the TLS loss than the crystal orientation of the TiN film and, consequently, the intrinsic material properties of the superconducting layer. The lowest TLS losses for all TiN depositions were achieved with a low power etch and low temperature resist strip. An additional buffered oxide etch (BOE) treatment could remove high-loss interfacial oxides at the metal-air (MA) and substrate-air (SA) interface and recover the etch-induced TLS losses. Consequently, TiN resonators exhibiting $\tildeδ_\mathrm{TLS}$ values as low as $9.67 \times 10^{-7}$ were realized. The corresponding median low-power loss, $\tildeδ_\mathrm{LP}$, amounts to $11.04 \times 10^{-7}$, which translates to an internal quality factor approaching one million. These findings highlight the critical role of process induced oxide formation at the MA and SA interfaces in limiting the performance of TiN resonators and provide a scalable, low-loss process compatible with industry-grade 200\,mm CMOS qubit fabrication workflows.

quant-pharXiv:2603.00441•Applied Physics Reviews•Mar 3, 2026•2 citations

Low-loss α-tantalum coplanar waveguide resonators on silicon wafers: fabrication, characterization and surface modification

Daniel Pérez Lozano, Massimo Mongillo, X Piao +19 more

Abstract The performance of state-of-the-art superconducting quantum devices is currently limited by microwave dielectric loss at different interfaces. α -tantalum is a superconductor that has proven effective in reducing dielectric loss and improving device performance due to its thin low-loss oxide. Here, we demonstrate the fabrication of high-quality factor α -tantalum coplanar-waveguide resonators directly on pristine 300 mm silicon wafers over a variety of metal deposition conditions and perform a comprehensive material and electrical characterization study. Additionally, we apply a surface treatment based on hydrofluoric acid that allows us to modify different resonators surfaces, leading to a reduction in two-level system loss in the devices by a factor of three. This loss reduction can be entirely attributed to the removal of surface oxides. Our study indicates that large scale manufacturing of low-loss superconducting circuits should indeed be feasible and suggests a viable avenue to materials-driven advancements in superconducting circuit performance.

arXiv:2211.16437•Materials for Quantum Technology•May 14, 2024•39 citations
Two level systems (TLSs) are a major source of loss in superconducting devices, limiting the performance of qubits, detectors, and resonators. These defects arise from a range of sources, including surface oxides, crystal defects, as well as fabrication residues which are often difficult to remove. Using NbTiN coplanar waveguide resonators, we show that depositing and subsequently removing a solid neon film can significantly improve device performance. Analysis of the temperature and power dependence indicates that this enhancement arises from reduced TLS dissipation, which we attribute to the redistribution and removal of surface contaminants during neon deposition and evaporation. Atomic force microscopy images of contaminated hexagonal boron nitride flakes before and after neon exposure show that neon treatment can redistribute and remove surface residues. These results demonstrate a simple, non-destructive approach for mitigating TLS losses in superconducting devices and other sensitive materials that cannot withstand aggressive cleaning processes.
We demonstrate a substantial reduction in two-level system loss in tantalum coplanar waveguide resonators fabricated on high-resistivity silicon substrates through the use of an ultrathin titanium sacrificial layer. A 0.2nm titanium film, deposited atop pre-sputtered α-tantalum, acts as a solid-state oxygen getter that chemically modifies the native Ta oxide at the metal-air interface. After device fabrication, the titanium layer is removed using buffered oxide etchant, leaving behind a chemically reduced Ta oxide surface. Subsequent high-vacuum annealing further suppresses two-level system loss. Resonators treated with this process exhibit internal quality factors Qi exceeding an average of 1.5 million in the single-photon regime across ten devices, over three times higher than otherwise identical devices lacking the titanium layer. These results highlight the critical role of interfacial oxide chemistry in superconducting loss and reinforce atomic-scale surface engineering as an effective approach to improving coherence in tantalum-based quantum circuits. The method is compatible with existing fabrication workflows applicable to tantalum films, offering a practical route to further extending T1 lifetimes in superconducting qubits.
Abstract The performance of superconducting qubits is often limited by dissipation and two-level systems (TLS) losses. The dominant sources of these losses are believed to originate from amorphous materials and defects at interfaces and surfaces, likely as a result of fabrication processes or ambient exposure. Here, we explore a novel wet chemical surface treatment at the Josephson junction-substrate and the substrate-air interfaces by replacing a buffered oxide etch (BOE) cleaning process with one that uses hydrofluoric acid followed by aqueous ammonium fluoride. We show that the ammonium fluoride etch process results in a statistically significant improvement in median T 1 by ∼ 22 % (p = 0.002), and a reduction in the number of strongly-coupled TLS in the tunable frequency range. Microwave resonator measurements on samples treated with the ammonium fluoride etch after niobium deposition and etching also show ∼ 33 % lower TLS-induced loss tangent compared to the BOE treated samples. As the chemical treatment primarily modifies the Josephson junction-substrate interface and substrate-air interface, we perform targeted chemical and structural characterizations to examine materials differences at these interfaces and identify multiple microscopic changes that could contribute to decreased TLS losses.
Materials imperfections in Nb -based superconducting quantum circuits—in particular, two-level-system (TLS) defects—are a major source of decoherence, ultimately limiting the performance of quantum computation and sensing. Thus, identifying and understanding the microscopic origin of possible TLS defects in these devices will help develop strategies that eliminate them, which are key to superconducting qubit performance improvement. In this paper, we demonstrate an order-of-magnitude reduction in two-level system losses in three-dimensional superconducting radio frequency (SRF) niobium resonators by a 10-h high vacuum (HV) heat treatment at 650 °C, even after exposure to air and high-pressure rinsing (HPR). X-ray photoelectron spectroscopy (XPS) and high-resolution scanning transmission electron microscopy (STEM) reveal an alteration of the native oxide composition regrown after air exposure and HPR and the creation of nanoscale crystalline oxide regions, which correlates with the measured tenfold quality factor enhancement at low fields of the 1.3 GHz niobium resonator. Tunneling spectroscopy measurements show a pronounced proximity effect that further confirms the presence of metallic layers on the niobium surface.
In current superconducting qubit circuit development, coherence time is limited by low-frequency flux noise introduced from localized two-level systems (TLSs) in the fabricated superconducting circuit, including superconducting materials, the interface between thin films, and the substrate. As a part of the effect to tackle this issue from a substrate standpoint, we succeed in fabricating NbN (200) oriented coplanar waveguide resonator (CPWR) on a thin titanium nitride (TiN) (200) buffered Si (100) substrate. The internal loss is close to 3 × 10-5nearphoton> ~1, improved from ~2 × 10-4in NbN (200) CPWR fabricated on MgO (100). For NbN (200) resonators grown on Si (100), the internal loss shows microwave energy independent. To further clarity if this energy independence is due to the change of substrate material, we also fabricated TiN (200) CPWR on Si (100). In contrast to NbN (200) CPWR, the loss of TiN (200) resonator shows a strong microwave dependent, an indication of TLSs originated from the interface and the surface. We suggest TLSs in NbN (200) CPWR are dominated from different mechanism other than arising from the interface and surface.
We report on the fabrication and characterization of superconducting coplanar waveguide (CPW) resonators based on titanium nitride (TiN) thin films deposited on 200\,mm diameter high-resistivity Si(100) substrates. We systematically investigate how deposition conditions, dry-etch power and in-situ resist strip temperature affect morphology, superconducting properties and dielectric losses. By tuning reactive sputtering conditions, three distinct preferred out-of-plane crystal orientations - (111), (200), and a mix of both are achieved. Our results demonstrate that all films exhibit similar minimal two-level system (TLS) losses, with TiN111 exhibiting the lowest median TLS losses δ~TLS\tildeδ_\mathrm{TLS}δ~TLS​, and greater robustness against reoxidation. The applied structuring process, in contrast, has a far greater influence on the TLS loss than the crystal orientation of the TiN film and, consequently, the intrinsic material properties of the superconducting layer. The lowest TLS losses for all TiN depositions were achieved with a low power etch and low temperature resist strip. An additional buffered oxide etch (BOE) treatment could remove high-loss interfacial oxides at the metal-air (MA) and substrate-air (SA) interface and recover the etch-induced TLS losses. Consequently, TiN resonators exhibiting δ~TLS\tildeδ_\mathrm{TLS}δ~TLS​ values as low as 9.67×10−79.67 \times 10^{-7}9.67×10−7 were realized. The corresponding median low-power loss, δ~LP\tildeδ_\mathrm{LP}δ~LP​, amounts to 11.04×10−711.04 \times 10^{-7}11.04×10−7, which translates to an internal quality factor approaching one million. These findings highlight the critical role of process induced oxide formation at the MA and SA interfaces in limiting the performance of TiN resonators and provide a scalable, low-loss process compatible with industry-grade 200\,mm CMOS qubit fabrication workflows.
Abstract The performance of state-of-the-art superconducting quantum devices is currently limited by microwave dielectric loss at different interfaces. α -tantalum is a superconductor that has proven effective in reducing dielectric loss and improving device performance due to its thin low-loss oxide. Here, we demonstrate the fabrication of high-quality factor α -tantalum coplanar-waveguide resonators directly on pristine 300 mm silicon wafers over a variety of metal deposition conditions and perform a comprehensive material and electrical characterization study. Additionally, we apply a surface treatment based on hydrofluoric acid that allows us to modify different resonators surfaces, leading to a reduction in two-level system loss in the devices by a factor of three. This loss reduction can be entirely attributed to the removal of surface oxides. Our study indicates that large scale manufacturing of low-loss superconducting circuits should indeed be feasible and suggests a viable avenue to materials-driven advancements in superconducting circuit performance.