N-doped 12C-enriched CVD diamond {111} freestanding crystals
Tokuyuki Teraji, Chikara Shinei, 増山 雄太
Abstract
Nitrogen concentration evaluated from electron paramagnetic resonance was 1 ppm. As shown in the birefringence image (Fig. 1(d)), it can be seen that crystal strain at the center of the freestanding crystal is smaller, while it is relatively high at both edges. Average coherence time T2* were 2.8 μs at the center and 0.4 μs at the edges, meaning that strain affect T2*.