Science China Physics Mechanics and Astronomy

Terahertz superconducting kinetic inductance detectors demonstrating photon-noise-limited performance and intrinsic generation-recombination noise

Qing Shi, Jing Li, Qiang Zhi, Zheng Wang, Wei Miao, Sheng‐Cai Shi

Published Jan 11, 2022• 14 citations
Publisher
DOI
10.1007/s11433-021-1828-y

Related papers

Terahertz Detectors Based on Superconducting Kinetic Inductance | NIST

Erich N. Grossman, Donald G. McDonald, Joseph E. Sauvageau

•Feb 1, 1991•1 citation

Demonstration of an NEP of 3.8×10−19 W/Hz1/2 at 1.54 THz in multiplexible superconducting microresonator detectors

Pieter de Visser, J. J. A. Baselmans, Juan Bueno +1 more

Microwave kinetic inductance detectors (MKIDs) promise high sensitivity, combined with device simplicity and intrinsic multiplexibility. We have measured the response and noise equivalent power (NEP) of an all-aluminium, antenna coupled MKID at 1.54 THz, both as a function of radiation power and as a function of readout power. Eight optical filters and a box-in-box configuration at the bath temperature, allow a large range of optical powers by varying the temperature of a black body source. In the range of 80 aW-700 fW the detector is photon-noise limited, with an optical efficiency of 48±8% for one polarisation, which is limited by the antenna design. At lower optical powers we reveal a saturation level in the NEP of 3.8×10-19W/Hz1/2, competitive with other detectors for this purpose and the lowest optical NEP so far for MKIDs. The noise over the entire power range is limited by photon- and generation-recombination noise, the fundamental noise sources for these detectors.

International Conference on Infrared, Millimeter, and Terahertz Waves (IRMMW-THz)•Sep 1, 2014•3 citations

Noise Optimization for MKIDs With Different Design Geometries and Material Selections

Zhaodi Pan, K. R. Dibert, J. Zhang +13 more

The separation and optimization of noise components is critical to microwave-kinetic inductance detector (MKID) development. We analyze the effect of several changes to the lumped-element inductor and interdigitated capacitor geometry on the noise performance of a series of MKIDs intended for millimeter-wavelength experiments. We extract the contributions from two-level system noise in the dielectric layer, the generation-recombination noise intrinsic to the superconducting thin-film, and system white noise from each detector noise power spectrum and characterize how these noise components depend on detector geometry, material, and measurement conditions such as driving power and temperature. We observe a reduction in the amplitude of two-level system noise with both an elevated sample temperature and an increased gap between the fingers within the interdigitated capacitors for both aluminum and niobium detectors. We also verify the expected reduction of the generation-recombination noise and associated quasiparticle lifetime with reduced inductor volume. This study also iterates over different materials, including aluminum, niobium, and aluminum manganese, and compares the results with an underlying physical model.

arXiv:2304.01133•IEEE Transactions on Applied Superconductivity•Mar 1, 2023•5 citations

Development of ultra high sensitivity superconducting THz detectors

李 婧 LI Jing, 张 文 ZHANG Wen, 缪 巍 MIAO Wei +1 more

Chinese Optics•Jan 1, 2017•5 citations

Development of high-Q superconducting resonators for use as Kinetic Inductance detectors

J. J. A. Baselmans, R. Barends, S. J. C. Yates +4 more

36th COSPAR Scientific Assembly•Jan 1, 2006•1 citation

Ultrasensitive hot-electron kinetic-inductance detectors operating well below the superconducting transition

Andrei V. Sergeev, Vladimir Mitin, Boris S. Karasik

While most experimental studies of kinetic-inductance sensors have been limited so far by the temperature range near the superconducting transition, kinetic-inductance detectors can be very sensitive at temperatures well below the transition, where the number of equilibrium quasiparticles is exponentially small. In this regime, a shift of the quasiparticle chemical potential under radiation results in the change of the kinetic inductance. We modeled the noise characteristics of the kinetic-inductance detectors made from disordered superconducting Nb, NbC, and MoRe films. Low-phonon transparency of the interface between the superconductor and the substrate causes substantial retrapping of phonons providing high quantum efficiency and the operating time of ∼1 ms at ≈1 K. Due to the small number of quasiparticles, the noise equivalent power of the detector determined by the quasiparticle generation–recombination noise can be as small as ∼10−19 W/Hz at He4 temperatures.

Applied Physics Letters•Feb 4, 2002•89 citations
Microwave kinetic inductance detectors (MKIDs) promise high sensitivity, combined with device simplicity and intrinsic multiplexibility. We have measured the response and noise equivalent power (NEP) of an all-aluminium, antenna coupled MKID at 1.54 THz, both as a function of radiation power and as a function of readout power. Eight optical filters and a box-in-box configuration at the bath temperature, allow a large range of optical powers by varying the temperature of a black body source. In the range of 80 aW-700 fW the detector is photon-noise limited, with an optical efficiency of 48±8% for one polarisation, which is limited by the antenna design. At lower optical powers we reveal a saturation level in the NEP of 3.8×10-19W/Hz1/2, competitive with other detectors for this purpose and the lowest optical NEP so far for MKIDs. The noise over the entire power range is limited by photon- and generation-recombination noise, the fundamental noise sources for these detectors.
The separation and optimization of noise components is critical to microwave-kinetic inductance detector (MKID) development. We analyze the effect of several changes to the lumped-element inductor and interdigitated capacitor geometry on the noise performance of a series of MKIDs intended for millimeter-wavelength experiments. We extract the contributions from two-level system noise in the dielectric layer, the generation-recombination noise intrinsic to the superconducting thin-film, and system white noise from each detector noise power spectrum and characterize how these noise components depend on detector geometry, material, and measurement conditions such as driving power and temperature. We observe a reduction in the amplitude of two-level system noise with both an elevated sample temperature and an increased gap between the fingers within the interdigitated capacitors for both aluminum and niobium detectors. We also verify the expected reduction of the generation-recombination noise and associated quasiparticle lifetime with reduced inductor volume. This study also iterates over different materials, including aluminum, niobium, and aluminum manganese, and compares the results with an underlying physical model.
While most experimental studies of kinetic-inductance sensors have been limited so far by the temperature range near the superconducting transition, kinetic-inductance detectors can be very sensitive at temperatures well below the transition, where the number of equilibrium quasiparticles is exponentially small. In this regime, a shift of the quasiparticle chemical potential under radiation results in the change of the kinetic inductance. We modeled the noise characteristics of the kinetic-inductance detectors made from disordered superconducting Nb, NbC, and MoRe films. Low-phonon transparency of the interface between the superconductor and the substrate causes substantial retrapping of phonons providing high quantum efficiency and the operating time of ∼1 ms at ≈1 K. Due to the small number of quasiparticles, the noise equivalent power of the detector determined by the quasiparticle generation–recombination noise can be as small as ∼10−19 W/Hz at He4 temperatures.