arXiv:2611.16015
The importance of shear strain in narrow Si/SiGe quantum wells
Hudaiba Soomro, Talise Oh, M. A. Eriksson, Benjamin D. Woods, Mark Friesen
Abstract
Several heterostructure profiles have been proposed for Si/SiGe quantum wells, to improve the operation of quantum-dot spin qubits. These structures share a common goal of generating either of the two wave vectors that govern the conduction-band valley coupling, dubbed $k_0$ and $k_1$. Here, we focus on the long-wavelength $k_1$ term that couples valleys when paired with shear strain, and which governs the Dresselhaus spin-orbit coupling. We show that shear strain induced by metal top gates may be enough to activate the $k_1$ valley-coupling mechanism, mitigating the need for "ultrasharp" interfaces, as commonly assumed for large valley energy splittings. We propose a scheme featuring narrow quantum wells that does not require ultrasharp interfaces, but should still provide large deterministic valley splittings (when paired with shear strain), and large spin-orbit couplings and $g$-factor corrections, which are of great interest for experimental implementations.
AI Summary
The paper asks whether shear strain can produce large, reproducible valley splittings in Si/SiGe spin-qubit quantum wells without ultrasharp interfaces. It studies a previously proposed strain-assisted mechanism that combines lattice deformation with confinement features at wave vector $2k_1$, corresponding to a length scale of approximately $1.6$–$1.7$ nm, rather than the conventional $2k_0$ scale of $0.33$ nm. Finite-element mechanical simulations of tungsten-gate devices are combined with a one-dimensional effective-mass model and statistical alloy-disorder calculations. For modeled gates aligned along [110], depositional stresses of $1.12$ and $4$ GPa yield shear strains around $0.15$–$0.5\%$ beneath plunger gates; corresponding [100]-aligned devices produce nearly zero shear strain along the studied linecuts. A $2.04$ nm well with $0.54$ nm interfaces gives deterministic valley splittings of $0.33$ and $0.88$ meV at strains of $0.17\%$ and $0.46\%$, respectively. Including alloy disorder, increasing strain suppresses low-splitting regions and narrows valley-phase distributions. The same confinement features enhance calculated Dresselhaus coupling to approximately $0.43$ meV nm and the intervalley $g$-factor correction magnitude to $0.042$. These are simulation predictions, not experimental demonstrations. The device geometry and layer stack are partly assumed because experimental specifications are unavailable, while depositional stresses depend on fabrication conditions. Oxide depositional stresses are neglected. Narrow wells increase alloy overlap and disorder, and diagonal strain components introduce substantial confinement-potential variations. The paper calls for experimental characterization of strain and its effects.
Written by gpt-6.1-sol from the paper's full text. Automated: it can be wrong.
- Comments
- 22 pages, 12 figures